Add to Cart
Corundum bricks include fused cast corundum brick, fused alumina
corundum brick and sintered corundum brick. fused cast corundum
brick is manufactured with commercial alumina and little sodium
carbonate and quartz powder fusing in the quartz powder and through
process of casting and annealing, and then form the shape and size
through machining.
Fused alumina corundum brick is made of fused alumina particle and
fines adding little fireclay and binding agent through molding by
brick machine after mulling. The refractory corundum brick is fired
in the temperature of 1700~1800℃ after drying .Corundum fire brick
is good quality high temperature refractory product. Corundum
fireproof brick has high refractoriness and good chemical
stability. Because corundum firebrick is manufactured with corundum
as the principal crystalline phase and contain more than 90%
alumina content. Corundum can not only resist acid and alkaline
slag erosion, but also the metal and glass liquid strongly.
Applications of Corundum Firebrick:
●Hot Blast Stove
●Refining Furnace
●Glass Furnace and blast Furnace
●Petrochemical Industrial Furnaces
●All kinds of high temperature kiln lining in metallurgical
industry
Advantages of CH series Corundum Firebrick:
●Low apparent porosity
●Wear-resisting property
●Good high temperature bending strength
●slag resistance, good thermal shock resistance
●Free sample,Free construction guidance ,free 3D design
●Customerize mould according to different size requirements for
free
Brand | CH-DL-95 | CH-DL-90 |
Al2O3 /% ≥ | 95 | 90 |
SiO2/% ≤ | 3.0 | 9.0 |
Fe2O3/% ≤ | 0.2 | 0.5 |
R2O /% ≤ | 0.6 | 0.6 |
Bulk Density g/cm3 ≥ | 2.9 | 2.9 |
Cold Crushing Strength / MPa≥ | 100 | 100 |
Refractoriness / ℃ ≥ | 1790 | 1790 |
Deformation Temperature 0.2MPa ℃/ ≥ | 1650 | 1650 |
Linear Change On Reheating 1600*3h /%≤ | 0.2 | 0.2 |
Thermal Stability (1100℃) /Times≥ | 1.0 | 1.0 |