OEM Hot Runner Typical Injection Molding Defects Analysis And Solutions - injectionmolded-parts

OEM Hot Runner Typical Injection Molding Defects Analysis And Solutions

Brand Name:OEM
Certification:ISO
Minimum Order Quantity:100pcs
Delivery Time:30day
Payment Terms:T/T
Price:Negotiable
Contact Now

Add to Cart

Site Member
Location: Dongguan Guangdong China
Address: Room 101, Building 1, No. 8, Hongying Erheng Road, Fenggang Town, Dongguan City, Guangdong Province
Supplier`s last login times: within 35 hours
Product Details Company Profile
Product Details

The Cause And Countermeasure Of Product Leaving Marks

Current Ripple


When the material in the mold is solidified and the molten material after the flow is mixed, such as Mi is not fully integrated, there will be dim and scaly in the product. Iridescent or ring shaped, this phenomenon is the flow mark, usually occurs at a slow speed


CauseCuntermeasure
Forming condition

1. The material overflow degree is too low, and the front section is very easy to cure

2. Mold temperature is too low

3. The speed of chaos molding is too fast or too slow, which will produce ripple flow marks when it is too slow and jagged flow marks when it is too fast

4. The filling pressure or holding pressure is too low, so that the flow mark is clear

show

1. Increase the molding temperature

2. Increase die temperature

3. Set the right speed

4. Increase filling and retaining pressure


Die

1. The gate is too small

2. No cold feed well

3. Improper pouring U position


1.F pour n

2. Open more cold feed Wells.

3. If pouring U is not fixed, the material will also touch the position of trapping mold hole wall

Product Design

1. Product structure design makes more right angles

2. The product is broken and the thickness difference is too large

1. Improve product shape and smooth molten material flow

2. Change the design to make the thickness too smooth

Material

1. Poor liquidity of materials

2. Too much filler


1. Improve liquidity

2. Switch to materials with fewer fillers

OtherBlockage of suona on injection molding machine

Clean the nozzle of the machine


China OEM Hot Runner Typical Injection Molding Defects Analysis And Solutions supplier

OEM Hot Runner Typical Injection Molding Defects Analysis And Solutions

Inquiry Cart 0