Superalloy Castings Parts Cobalt Alloy Castings Parts Nozzle With Wax Lost Process

Brand Name:Eternal Bliss
Certification:ISO9001-2008
Model Number:EB9064
Minimum Order Quantity:30kg
Delivery Time:It depends on the quantity to be ordered.
Payment Terms:by T/T or L/C, Western Union
Contact Now

Add to Cart

Active Member
Location: Wuxi Jiangsu China
Address: 1099 Xinhua Road,214104, Xishan District, Wuxi, Jiangsu,China
Supplier`s last login times: within 1 hours
Product Details Company Profile
Product Details

Cobalts Alloy Castings Parts Nozzle with Wax Lost Process EB9064

We produce High Temperature Superalloy Castings Parts with centrifugal cast process, investment process and resin sand cast process.
We melt good quality Co-based Alloy Castings with Vacuum Furnaces and Induction Furnaces.
We can cast and machine the hard Cobalt-based Alloy Castings as per the drawings.
We would like to help select suitable Co-based Alloy Grade as per your specific working condition.

Cobalt-based alloys have been in use for producing various components such as vanes or combustion chambers. The material can be implemented as wrought or as precision-cast parts or as centrifugal cast parts. The design of cobalt superalloys, which is aimed at an enhancement of both their oxidation resistance and their hot corrosion resistance, has received considerable impetus recently, especially since the advent of overlay coating techniques and the extensive studies which have been undertaken to elucidate the hot corrosion mechanisms and the effect of alloying elements.


Table 1 : Standard Cobalt & Nickel Base Alloys

cobalt alloy Alloy Overlay Welding

CoCrCWMoNiSiBFeMnOthers
cobalt alloy 1BAL332.4513-2.5*1-2.5*1-
cobalt alloy 3BAL312.513-2.5*1-2.5*1-
cobalt alloy 4BAL31.5114-2.0*1-2.0*1-
BAL281.25-3.0*1-2.5*1-
cobalt alloy 12BAL291.859-2.5*1-2.5*1-
cobalt alloy 20BAL332.4517.5-2.5*1-2.5*1-
cobalt alloy 21BAL270.25-5.52.5*1-3.0*1-
cobalt alloy 31BAL260.57.5-10.51-2.0*1-
cobalt alloy 190BAL263.314-1.01-8.00.5-
cobalt alloy 238BAL260.1-3-1-20.01-
cobalt alloy 306BAL250.42-6.01-4.0*1Nb=5
94BAL28119-5.01-2.5*1V=1
cobalt alloy FBAL25.51.7512.25-22.51-1.5*--
cobalt alloy SF1BAL191.313-1332.53*0.5Cu=0.5
cobalt alloy SF6BAL190.77-132.51.73*0.5Cu=0.5
cobalt alloy SF12BAL1919-13323*0.5Cu=0.5
cobalt alloy SF20BAL191.515-13332*0.5Cu=0.5
TRIBALOY T400BAL80.1*-283*2.4-3*--
TRIBALOY T800BAL170.1*-283*3.2-3*--
DELORO 15--0.06*--BAL2.01.051.5*20Cu=20
DELORO 22-0.700.10--BAL2.31.75---
DELORO 40-7.00.10--BAL3.52.25---
DELORO 50-10.250.45--BAL4.01.854.0--
DELORO 60-14.250.6--BAL2.03.54.0--
DELORO 625-220.1-9BAL--5--
NISTELLE C-16.50.12*4.517BAL0.7-6.0--
TRIBALOY T700-150.10*-32BAL3.25-
Hastelloy C22®(UNS N06022)(Max.)
CMNPSSiCrNiMoCOFeWV
0.0150.50.020.020.0820.0-22.5Bal.12.5-14.52.52.0-6.02.5-3.50.35
Hastelloy C276®(UNS N10276)(Max.)
CMNPSSiCrNiMoCOFeWV
0.0110.040.030.0814.5-16.5Bal.15.0-17.02.54.0-7.03.0-4.50.35
Hastelloyx®(UNS N06002)(Max.)
CMNPSSiCrNiMoCOFeWother
0.05-0.1510.040.03120.5-23.0Bal.8.0-10.00.5-2.517.0-20.00.2-1.0/
Monel 400®(UNS NO4400) (Max.)
CMNSSiNiCuFe
0.320.0240.563 min28-342.5
Monel M400®(UNS NO4400)(Max.)
CMNSSiNiCuFe
0.320.0240.563-7028-342.5
Monel R405®(UNS NO4405)(Max.)
CMNSSiNiCuFe
0.320.025-0.060.563.0min28-342.5
Monel K500®(UNS NO5500)(Max.)
CMNSSiNiCuTiAIFe
0.120.010.563min27-330.862.3-3.152
Inconel 600(UNS NO6600)(Max.)
CMNSSiCrNiCuFe
0.1510.0150.514-1772 min0.56.0-10.0
Inconel 601(UNS NO6601)(Max.)
CMNSiCrNiCOAIFe
0.050.30.222.561.5min51.414.1
Inconel 718(UNS NO7718)(Max.)
CrNiMoCOCb+TaTiAIFe
1952.5min3.0555.130.90.518.5
Chemical Analysis of Incoloy 800® uns(N08800)
CCrNiTiAIFeGrain
0.1 max19.0-23.030.0-35.00.15-0.60.15-0.639.5min/
Incoloy800H® UNS(N08810)
CCrNiTiAIFeGrain
0.05-0.119.0-23.030.0-35.00.15-0.600.15-0.6039.5min5or coarser
Incoloy800HT® UNS(N08811)
CCrNiTiAIFeGrain
0.06-0.1019.0-23.030.0-35.00.25-0.600.25-0.6039.5min5or coarser


Production Process


Step 1: Getting orders.


Step 2: Process design by technical department


Step 3: Purchase of raw materials and pattern making &checking


Step 4: Inspection of raw materials


Step 5: Melting by middle-frequency induction furnaces


Step 6: Ladle analysis by Spectrometer


Step 7: De-oxidization, slag-removal, tapping


Step 8: Pouring


Step 9: Openning & fettling


Step 10: Surface & dimensional check


Step 11: Heat treatment


Step 12: Inspection of physical property (UT test,MT test, hardness,impact value µstructure)


Step 13: Packing


Step 14: Shipping



China Superalloy Castings Parts Cobalt Alloy Castings Parts Nozzle With Wax Lost Process supplier

Superalloy Castings Parts Cobalt Alloy Castings Parts Nozzle With Wax Lost Process

Inquiry Cart 0