OEM 7079 Forging Aluminum Parts For Skeleton Large Forgings/Spare Parts/Die Forged
Product Details
Material | Aluminum Alloy 7079 |
Process | Forging+CNC+Heat Treatment |
Surface Treatment | Transparent, Color Anodized, Hard Anodizing, Powder Coating; |
Manufacture Ability | Depends on The Complexity Of Different Products And Quantities |
Experience | Aluminum Machining Service for 12 Years |
Packaging | Standard Export Wooden Pallets |
MOQ | 1pcs |
Sample | Can Be Customized |
Mold | Can Be Customized |
Lead Time | Mold for 15-20 Days Process for 15-20 Days |
OEM | Can Be Customized |
Chemical Composition of 7079 | |||||||||||||
Alloy | Si | Fe | Cu | Mn | Mg | Cr | Zn | Ti | Others | Al | |||
Each | Total | ||||||||||||
7079 | 0.30max | 0.40max | 0.40-0.80 | 0.10-0.30 | 2.90-3.70 | 0.10-0.25 | 3.80-4.80 | 0.10max | 0.05max | 0.15max | Rest |
Technical Specifications of 7079
7079 Aluminum Mechanical Properties
Hardness, Brinell | 150 | 150 | AA; Typical; 500 g load; 10 mm ball |
Hardness, Knoop | 191 | 191 | Converted from Brinell Hardness Value |
Hardness, Rockwell A | 53.5 | 53.5 | Converted from Brinell Hardness Value |
Hardness, Rockwell B | 87 | 87 | Converted from Brinell Hardness Value |
Hardness, Vickers | 175 | 175 | Converted from Brinell Hardness Value |
Ultimate Tensile Strength | 572 MPa | 83000 psi | AA; Typical |
Tensile Yield Strength | 503 MPa | 73000 psi | AA; Typical |
Elongation at Break | 11 % | 11 % | AA; Typical; 1/16 in. (1.6 mm) Thickness |
Elongation at Break | 11 % | 11 % | AA; Typical; 1/2 in. (12.7 mm) Diameter |
Modulus of Elasticity | 71.7 GPa | 10400 ksi | AA; Typical; Average of tension and compression. The compression modulus is about 2% greater than tensile modulus. |
Poisson’s Ratio | 0.33 | 0.33 | |
Fatigue Strength | 159 MPa | 23000 psi | AA; 500,000,000 cycles completely reversed stress; RR Moore machine/specimen |
Fracture Toughness | 20 MPa-m½ | 18.2 ksi-in½ | K(IC) in S-L Direction |
Fracture Toughness | 25 MPa-m½ | 22.8 ksi-in½ | K(IC) in T-L Direction |
Fracture Toughness | 29 MPa-m½ | 26.4 ksi-in½ | K(IC) in L-T Direction |
Machinability | 70 % | 70 % | 0-100 Scale of Aluminum Alloys |
Shear Modulus | 26.9 GPa | 3900 ksi | |
Shear Strength | 331 MPa | 48000 psi | AA; Typical |
7079 Aluminum Thermal Properties
CTE, linear 68°F | 23.6 µm/m-°C | 13.1 µin/in-°F | AA; Typical; Average over 68-212°F range. |
CTE, linear 250°C | 25.2 µm/m-°C | 14 µin/in-°F | Average over the range 20-300ºC |
Specific Heat Capacity | 0.96 J/g-°C | 0.229 BTU/lb-°F | |
Thermal Conductivity | 130 W/m-K | 900 BTU-in/hr-ft²-°F | AA; Typical at 77°F |
Melting Point | 477 – 635 °C | 890 – 1175 °F | AA; Typical range based on typical composition for wrought products 1/4 inch thickness or more significant. Homogenization may raise the eutectic melting temperature by 20-40°F but usually does not eliminate eutectic melting. |
Solidus | 477 °C | 890 °F | AA; Typical |
Liquidus | 635 °C | 1175 °F | AA; Typical |