Add to Cart
CORILON SL-W200/M100 water based industrial Coatings , it is idea
for rubber mould , plastic mould , shoe molds, Cup bevel, EVA mold,
glove mold, absorb mold, EPS foam mold ect.
Also use for textile industry series: roller machinery of textile
and leather, roller embossing, gluing roller gluing, copier roller,
dyeing and finishing roller, warp sizing roller, non-woven fabric
roller and other parts, With quality to be on a par with
internation famous brand, one step finished coat’s usage can reach
1 year around.
CORILON SL-W200/M100 Operate instruction:
Water based coating flux (Waterborne Fluororesin coating) as a two
component fluorocarbon coating flux, excellent inadhesion and
wearing property, but the step for operating stages is very strict
with requirements, read booklet carefully before putting it to use.
▲. Material treatment:
Dry-boiling for the material like aluminum and stainless steel in
30 minutes by 380℃ temperatures firstly or dissolvent to cleaning
the first step’s degreasing, and goes on with roughening for
surface of subject in next step, utilizing the steel jade sand
No.:80~100, 0.4mpa~0.6mpa compressive stress, sand thickness:
2.0μm~3.5μm.
▲. Spray SL-M100 priming coating:
Rolling about 120 rotation per minute, no less than 2.0 hours at a
time before putting the priming coating to use, no less than once
time every week for rolling it up. Keep flat for the having been
handled the material( material must be unsmirched, dried, not
included celvacene greases and pollutional, it will have a strong
impact on the adhesive attraction or cause the decrustation go so
far as do if touch the sand’s surface by hand).
Applied diameter:
1.0mm~1.5mm ejection gun to have transferred into the compressive
stress: 0.20mpa~0.3mpa keeping distance: 20cm~30cm; If spray
coating directly, adopting the 150℃ temperatures to task in 15
minutes~20minutes, thickness of dry film approximately 10μm~15μm
after having it been dried.
▲. Spray finishing of SL-W200 top coating ( μm ):
Rolling about 100 rotation per minute with the slow speed, no less
than 3.0 hours at a time and mixed it up equably absolutely before
putting the top coat to use. The top coating will be painted after
the having been coated priming paint workpiece has cooled off the
normal atmospheric temperature (The surface must be unsmirched
absolutely and unpolluted. thickness of dry film approximately
10μm.
▲ Re-spray SL-W200 Top coating,
Applied diameter:
1.0MM ~1.5MM of the ejection gun to have transferred into the
compressive stress:0.20mpa~0.30mpa, keeping 20cm~30cm distance;
adopting the 150℃ temperatures in 10 minutes~15minutes to task
until dried, then adopt 400℃ temperatures to having been sintered
in 10 minutes or so, the total thickness of having been sintered
dry film: 25±3μm approximately. (The sintered insufficiency will
have an effect on the adhesivity and reduce physical
characteristics of coat, but the sintered immoderateness will cause
the variation of rate of coat functions, be cautious in
performance! )
▲ Re-spray SL-W200 Top coating.
If you need more high gloss, after the first step Spray finishing
of SL-W200 top coating, please make polishing with water and
rubber, then spray SL-W200 Top coating again, the gloss, useful
life and non ticky will be improved , The sintered coating can
survive long-term use at temperatures up to 170℃, but use at higher
temperatures is not recommended.