Fused Silica Fused Quartz Wafer

We specialize in fabricating series of glass materials, including fused quartz, synthetic quartz, borosilicate glass, sodium calcium glass, low expansion glass, low alkali glass, etc., covering infrared, visible light, ultraviolet multiple bands, can be processed into excellent optical window material, base plate, etc.


Material Brand

Schott

Borofloat33 / BK7 / B270 / D263 etc.

Corning

Eagle XG , Fused Silica 7980 / 7978 / 7979 etc.

Feilihua

Fused Silica JGS1 / JGS2 & Single quartz etc.

Ohara

SK-1300

GM

H-K9L / Soda Lime etc.


Processing Capacity

Specification

unit3”4”5"6"8"12"
Diameter (or Square)mm76.2100125150200300
Tol(±)mm<0.1~0.25 mm
Thinnest Thicknessmm>0.10>0.18>0.30>0.30>0.30>0.50
Primary Flatmm2232.542.557.5/notchnotchnotch
LTV (5mmx5mm)µm<2<2<2<2<2<10
TTVµm<5<5<5<5<10<10
Bowµm±15±20±30±60±60±60
Warpµm<15<20<30<40<70<70
PLTV(<0.5um)%≥95%(5mm*5mm)
TransmittanceUV, Optical, IR or Custom option
Edge RoundingmmCompliant with SEMI M1.2 Standard/refer to IEC62276
Surface TypeSingle Side Polished / Double Sides Polished
Polished side Ranm<1.0nm or per requested
Back Side CriteriaµmGeneral is 0.2-0.5µm or as customized
AppearanceContaminationNone
Particles >0.3µm<=30
Saw Marks, striationsNone
ScratchNone
Cracks, crowsfeel saw marks, stainsNone



Acceptance Check


1. The product is fragile. We have adequately packed it and labeled it fragile. We deliver through excellent domestic and international express companies to ensure transportation quality.


2. After receiving the goods, please handle with care and check whether the outer carton is in good condition. Carefully open the outer carton and check whether the packing boxes are in alignment. Take a picture before you take them out.


3. Please open the vacuum package in a clean room when the products are to be applied.


4. If the products are found damaged during courier, please take a picture or record a video immediately. DO NOT take the damaged products out of the packaging box! Contact us immediately and we will solve the problem well.

China 0.05mm To 10mm Fused Silica Fused Quartz Wafer JGS1 JGS2 JGS3 supplier

0.05mm To 10mm Fused Silica Fused Quartz Wafer JGS1 JGS2 JGS3

Inquiry Cart 0