Add to Cart
PP Fiber Twisted Bunchy form
Polypropylene Fiber (PP Fiber) is made from 100% virgin PP granular, after extruding from different mould and technology, we can get 4 different types of fiber, including Monofilament form, Fibrillated Mesh form, Twisted Bunchy and Wave form with different size. These fiber can improve the reinforcement of mortar or concrete performance effectively to make them strong and protect the projects.
Product Description
1. This fibre is used to instead of steel fiber for reinforcement
to cement concrete.
2. The rigid polymer fibre is used polypropylene as its raw
material, produced the rough surface treatment by special parallel
thread extruding & twisting process. It has high break
strength, better dispersion and strong combining ability, will be
widely used to instead of steel fibre to
reinforce the cement concrete and crack-resistant.
APPLYING INSTRUCTION:
1. Ration design of the fibre concrete:
Generally the recommended amount to add to the concrete is more
than 2.7kg per sqm (volume ratio is 0.3%), reinforcement adding
amount is
5.5kg, Compared with adding 47kg of steel fibre, 5.4kg polymer
fibre has the same volume ratio to the concrete.
2. Length: 54mm for common crack-resistant requirement.
3. Matching Ratio:
Usually, it is no need to Change the matching ratio of the
concrete. Considering the requirement of fissure-resistant, the
polymer fiber is recommend to combine with the PP fiber mesh form
with the volume ratio of 1:1(0.9kg fiber-mesh to per sqm of cement
concrete). .
4. Mixer Adoption:
Double-axle horizontal compelling mixer is priority.
5. Mixing process:
Crushed stones, fibers and sands are put into the mixer in
succession. After stirring for two minutes, fiber will fully spread
and then add cement and water and stir normally. The addition of
materials also can be put into as common concrete, but the stirring
time should be properly prolonged to make fiber com-pletely mixed.
6. Shaping & Maintenance:
There is no special requirement, may along the vibrating time for
30s, The maintenance of the fibre concrete should be done same as
the normal
concrete.
Resist to shrink & crack | Increase seepage resistance |
Increase friction resistance | Increase freezing & thawing resistance |
Improve tendons protection | Replace steel net (using in plastering) |
Prevent mortar split and crackle expansion | Increase impact resistance and peeling resistance |
Specification
Raw material | PP+PE |
Modulus (Mpa) | 5000min |
Fiber Length (mm) | 54 |
Density | 0.91g/cm3 |
fiber diamter | 0.3±0.05 |
acid&alkali resistance | Excellent |
Break tensile ratio | 15%min |
Break strength (Mpa) | 560min. |
Application:
1. The surface of road, bridge, runway and floor of the factory.
2. Wall and roof of the tunnel and mine.
3. Dam, river, bridge pier, dock and military protection
facilities.
Packing
1kgs per bag, 10kgs per carton.
Quantity: 400CTNS/20`FCL;
828CTNS/40`FCL;
930CTNS/40`HQ
Packing image: