2.4851 Inconel Alloy Inconel 601 Pipe UNS N06601 Nickel Based Superalloys

Brand Name:ABOOM
Certification:EN 10204 Type 3.1
Model Number:Inconel 601
Minimum Order Quantity:1000kgs
Delivery Time:7-15dyas
Payment Terms:T/T
Contact Now

Add to Cart

Active Member
Location: Shanghai Shanghai China
Address: NO.161 XingFei Road ,Songjiang Disrict,Shanghai 201601, P.R.CHINA
Supplier`s last login times: within 30 hours
Product Details Company Profile
Product Details

2.4851 Inconel Alloy Inconel 601 Pipe UNS N06601 Nickel Based Superalloys


Inconel 601 UNS N06601 nickel based alloy seamless pipe 2.4851


Material designation: Inconel 601 nickel based alloy

US grade: N06601

German grade: 2.4851


Inconel 601 (N06601) nickel-based alloy processing heat treatment:


Inconel 601 (UNS N06601) nickel-based alloy is not a precipitation hardening alloy, so it cannot be aged hardened by heat treatment. When the temperature after cold working reaches about 900 ° C, the material softens. If the material needs high-temperature strength, it is recommended that the solution heat treatment be performed at a temperature of 1100 to 1200 ° C. At this time, the cooling method is water cooling.

Depending on the thickness of the plate, air cooling can also be used. However, in order to avoid carbide precipitation, it is recommended to cool as quickly as possible in the temperature range of 500 to 800 ° C.


Inconel 601 (N06601) nickel-based alloy chemical composition: see Table-1:

Table-1 %

C≤Si≤Mn≤P≤S≤Cr≥Ni≥Mo≥Cu≤
0.100.501.000.0200.01521.0-25.072.01.00
OthersN≤Al≤Ti≤Fe≤Co≤V≤W≤Nb≤
1.00-1.70Balance

specification:


Outer diameter Φ6—762mm; wall thickness: 0.5-50mm, maximum length 18000mm
Special specifications are available upon negotiation.

China 2.4851 Inconel Alloy Inconel 601 Pipe UNS N06601 Nickel Based Superalloys supplier

2.4851 Inconel Alloy Inconel 601 Pipe UNS N06601 Nickel Based Superalloys

Inquiry Cart 0