Home /Rare Earth Magnets /

A2 SKD12 1.2363A2 Special Cold Work Die Steel

A2 SKD12 1.2363A2 Special Cold Work Die Steel

Brand Name:takford
Model Number:A2
Minimum Order Quantity:1 pc
Delivery Time:20-50 DAYS
Payment Terms:L/C, T/T, Western Union
Place of Origin:CHINA
Contact Now

Add to Cart

Verified Supplier
Location: Dongguan Guangdong China
Address: Postal code is 523196, No.8 shanghe precinct, wangniu dun town , dongguan city. Guangdong province China
Supplier`s last login times: within 27 hours
Shipping
lt's easy to get a shipping quote! Just click the button below and complete the short form.
Get Shipping Quote
Product Details Company Profile
Product Details

A2 COLD WORK TOOL STEEL, SPECIAL STEEL, DIE STEEL/SKD12/1.2363A2 DIE STEEL, SPECIAL STEEL, COLD WORK STEEL


Chemical composition

C(%)0.95~1.05Si(%)0.10~0.50Mn(%)0.40~1.00P(%)≤0.030
S(%)≤0.040Cr(%)4.75~5.50Mo (%)0.90~1.40V(%)0.15~0.50

Heat treatment Related

  • Forged of A2 Tool steel

Slowly heated the A2 steel material to 650-680°C (1202-1256°F) before raising the temperature to 1050-1100°C (1922-2120°F) and soak A2 tool steel material until uniformly heated. Initial hammer blows should be light due to the comparatively high hot strength of this steel.

The A2 steel forged temperature should be maintained above 1000°C(1832℉) until the A2 steel metal begins to yield. Final forged should not be done below 900°C(1652℉). Slowly cool after forged is essential to avoid the possibility of cracking.

  • Annealing of A2 Tool steel

Slowly heated A2 steel to 850-870 ℃(1562-1598°F) and allow enough times, let the steel to be thoroughly heated, Then cool slowly in the furnace at a rate of 4°C (40°F) per hour or less.. The A2 tool steel will get MAX 250 HB (Brinell hardness).

  • Hardening of A2 tool steel

A2 steels should be heated uniformly to 790-820°C (1436-1508°F) until completely heated through. Then heated to the hardening temperature of 950-980°C(1742-1796℉), soak at the temperature enough time, let A2 steel to be thoroughly heated .

Then withdraw A2 steel tools from the furnace,either air cool or oil quench.


Tempering of A2 tool steel

Tempering of A2 steels is performed at 150-400°C (302-752°F), Soak well at the selected temperature and soak for at least one hour per 25mm of total thickness. Get Rockwell C hardness of 57 to 62. Others different Heat treatment temperature will get different hardness. Below only for reference.

Temperature [℃] 150 200 250 300 350 400

Hardness [HRc] 62-61 61-60 60-59 59-58 58-57 58-57