1. Technological process of ABS plastic plating

degreasing → water washing → roughening → water washing → colloidal palladium activation → water washing → gel release → water washing → chemical nickel plating → water washing → nickel electroplating → water washing →copper electroplating→ water washing→ chrome electroplating→ water washingdrying


2. Main process introduction

2.1 Degreasing:remove oil and reducing its surface tension, endowing it with surface hydrophilicity.
2.2 Roughening:improve surface roughness and increase surface area to increase the adhesion between metal coatings and plastics; Make the plastic surface change from hydrophobic to hydrophilic, and all parts are evenly wetted with water to evenly adsorb metal ions.
2.3 Colloidal palladium activation:a layer of easily oxidized material is adsorbed on the surface of the product, so that Redox can occur during the activation treatment, and a precious metal film with catalytic effect can be formed on the surface of the product.
2.4 Gel release:generate a layer of palladium metal film on the surface of the product.
2.5 Chemical nickel plating:plating a layer of nickel on the surface of the workpiece to strengthen the conductive layer.
2.6 Electroplating:plating the required coating on the surface of the product.


3.Solution preparation

Pre-nickel plating solution: Ni(SO3NH2)2 400~600mL/L
NiCl2 5~15g/L
H3BO3 40~60g/L

Nickel plating solution: Ni(SO3NH2)2 400~600mL/L
NiCl2 5~15g/L
H3BO3 40~60g/L
Softening agent 8~12mL/L
Brightening agent 0.2~0.8mL/L

4.Common faults and solutions


Common faultsCause of occurrenceSolution
Pitted spotImpurities in electroplating waterUsing deionized water
Solid impurities in the electroplating bathStrengthen filtering
Excessive coarseningAdjusting the roughening process
PinholeUneven air stirring in electroplating tankImprove air stirring
Exposed plasticElectroplating tank contaminated with roughening solutionPrevent coarsening solution from entering the plating bath
Insufficient thickness of chemical nickel platingAdjust the nickel plating solution within the process range
YellowingChromium layer too thinIncrease chromium plating current
ScorchExcessive current in the local part of the productReduce current
RustPoor conductivity of hanging toolsMake a new hanging tool
Strong corrosive media present in the environmentimprove environment
BubblingPoor material performanceSelect electroplating grade ABS
Excessive or poor rougheningReduce or increase the coarsening level appropriately

5.Packaging & Shipping

We can pack it by pallet, or according to the customers' specific requirements.

Port: Shanghai/Ningbo


6. Our Services
In order to guarantee the customers are able fully to operate the machine, if the customer need, we can help customer training, includes:
(1) Correct operating mode
(2) Correct maintenance way
(3) Correct technological process control
(4) Remove simple problem
All the electroplating machine of our company have already been widely used in electroplating area.


Any doubt please contact us.


China Custom ABS Plastic Electroplating Machine PLC Control 220V / 50HZ supplier

Custom ABS Plastic Electroplating Machine PLC Control 220V / 50HZ

Inquiry Cart 0