Aluminum PCB has been widely used in hybrid integrated circuits, automobiles, office automation, high-power electrical equipment, power supply equipment and other fields in recent years with excellent heat dissipation, machinability, dimensional stability, and electrical properties. Aluminum substrate is mainly to see the thermal conductivity, voltage value and thermal resistance value, it is related to the life and life of aluminum substrate.
1. Aluminum PCB process flow:
Opening → Drilling → Dry film → Inspection → Etching → Exposure → Soulder mask → Silk screen → Inspection → Tin Spray → Aluminum surface treatment → Punching → Final inspection → Packaging → Shipping
3. Specific production process and special production parameters:
3.1 Opening
3.1.1 Strengthen the incoming inspection (the sheet with protective
film on the aluminum surface must be used).
3.1.2 No baking plate is required after opening.
3.1.3 Handle gently, pay attention to the protection of the aluminum base surface (protective film).
3.2 Drilling
3.2.1 The drilling parameters are the same as those of FR-4.
3.2.2 The aperture tolerance is extremely tight. The copper base of
4OZ needs to pay attention to controlling the generation of wave
peaks.
3.2.3 Drill holes with the copper skin facing up.
3.3 Dry film
3.3.1 Incoming inspection: Before grinding the board, the aluminum
base surface protective film must be inspected. If it is damaged,
it must be pasted with blue glue before pretreatment.
3.3.2 Milling: only the copper surface is processed.
3.3.3 Filming: Both copper surface and aluminum base surface must
be filmed.
Control the time between the grinding plate and the film to be less
than 1 minute to ensure that the film temperature is stable.
3.3.4 Clapper: Pay attention to the accuracy of the clapper.
3.3.5 Exposure: Exposure rule: 7 to 9 grids have residual glue.
3.3.6 Development: Pressure: 20 ~ 35psi, Speed: 2.0 ~ 2.6m / min
Each operator must be careful to avoid scratches on the protective film and aluminum substrate.
3.4 Inspection
3.4.1 The circuit surface must check each content according to MI
requirements.
3.4.2 The aluminum base surface must also be inspected. The dry film on the aluminum base surface must not have film falling and damage.
3.5 Etching
3.5.1 Because the copper base is generally 4OZ, there will be some
difficulties during etching. The first board must be approved by
the foreman before it can be used as a board. Spot checks on line
width and line gap should be strengthened in the board. The line
width should be checked every 10PNL board and recorded.
3.5.2 Recommended parameters: Speed: 7 ~ 11dm / min Pressure: 2.5kg
/ cm2
Specific gravity: 25Be Temperature: 55 ° C
(The above parameters are for reference only, subject to test
results)
3.5.3 When removing the film, pay attention to the time control between 4 ~ 6min, because aluminum and NaOH will react, but it must also ensure that the film is clean, and the film is not allowed to warm up during the film. After the board with no protective film on the aluminum surface is raised from the film release liquid, if the board cannot stay in time, the film release liquid on the plate needs to be washed with water to prevent the alkaline liquid from biting the aluminum surface.