275 MPa Molybdenum Heating Elements For Semiconductor Industry

Brand Name:Hypersolid Metal
Model Number:Molybdenum heating elements
Minimum Order Quantity:Negotiate
Delivery Time:30 days after receiving down payment
Payment Terms:D/A, L/C, D/P, T/T, Western Union, MoneyGram
Place of Origin:China
Contact Now

Add to Cart

Verified Supplier
Location: Luoyang China
Address: Luoyang National University Science and Technology Park
Supplier`s last login times: within 1 hours
Product Details Company Profile
Product Details

molybdenum heating elements molybdenum heater molybdenum crucibles


Description:


Molybdenum heating elements are heating components made from molybdenum, a refractory metal known for its high melting point and excellent thermal properties. Here are some descriptions of molybdenum heating elements:

  1. High melting point: Molybdenum heating elements have an exceptionally high melting point of approximately 2,620 degrees Celsius (4,748 degrees Fahrenheit). This property allows them to withstand extreme temperatures without melting or deforming, making them ideal for high-temperature heating applications.

  2. Excellent thermal conductivity: Molybdenum heating elements possess excellent thermal conductivity, allowing efficient heat transfer. They can quickly and evenly distribute heat, making them suitable for applications requiring precise and uniform heating, such as in high-temperature furnaces and industrial heating processes.

  3. Rapid heating and cooling capability: Due to their high thermal conductivity and low heat capacity, molybdenum heating elements offer rapid heating and cooling capabilities. They can heat up quickly and respond swiftly to changes in temperature, providing precise control over the heating process.

Specifications:


Chemical SymbolMo
Atomic Number42
Atomic Weight95.95 g/mol
Melting Point2,620 degrees Celsius (4,748 degrees Fahrenheit)
Boiling Point4,612 degrees Celsius (8,354 degrees Fahrenheit)
Density10.22 g/cm³
Crystal StructureBody-centered cubic
Electrical Conductivity27% IACS (International Annealed Copper Standard)
Thermal Conductivity138 W/m·K
Specific Heat Capacity0.251 J/g·K
Coefficient of Expansion5.1 x 10^(-6) K^(-1)
Young's Modulus329 GPa
Tensile Strength585-690 MPa
Elongation at Break10-30%
Hardness (Mohs)5.5