LRC-03 ISO 3187 High Temperature Rul and Creep Tester Refractoriness Under Load Tester - lab-testmachines

LRC-03 ISO 3187 High Temperature Rul and Creep Tester Refractoriness Under Load Tester

Brand Name:Lonroy
Certification:Includes Calibration Certification
Model Number:LRC-03
Minimum Order Quantity:1
Delivery Time:5-8 work days
Payment Terms:L/C,D/A,D/P,T/T,Western Union
Contact Now

Add to Cart

Verified Supplier
Location: Dongguan Guangdong China
Address: A31, 11 Floor, No 1 Building, Minjian Jinrong Building, No 111 Guantai Road, Sanyuanli Community, Nancheng Street, Dongguan, Guangdong, China
Supplier`s last login times: within 29 hours
Product Details Company Profile
Product Details

LRC-03 ISO 3187 High-Temperature Rul and Creep Tester Refractoriness Under Load Tester

1.Description:

This instrument is used to test the resistance of refractory materials under high-temperature and load softening conditions, which is an important indicator for evaluating the high-temperature mechanical properties of refractory materials. It complies with the national standards GB/T5073-2005 "Test Method for Creep of Refractory Materials under Pressure" and GB/T5989-2008 "Test Method for Softening Temperature under Load of Refractory Materials". It is equipped with a computer for automatic testing and data processing, automatically generating and saving the temperature and deformation curve graphs.
2.Configuration:
Includes 1 LRC testing instrument main unit, 1 testing software, 1 set of communication interface and data cable, 1 high-temperature test column, 1 high-temperature test column, 1 B-type thermocouple, 1 set of silicon molybdenum rods, 1 set of weights, and 1 desktop computer (configured according to the contract).

3.Technical Parameter

ParameterSpecification
Operating TemperatureRUL Test: 1700°C
Creep Test: 1550°C
Heating Rate0-10°C/min adjustable
Temperature Control Accuracy±1°C
Temperature Uniformity±10°C
Deformation Measurement Range0-10 mm
Deformation Accuracy0.1% FS (Full Scale)
Load Range0.05-0.2 MPa
Continuous Samples3 specimens
Heating ElementsMolybdenum Disilicide (MoSi2) Rods
ThermocoupleType B (Pt-Rh/Pt-Rh)
China LRC-03 ISO 3187 High Temperature Rul and Creep Tester Refractoriness Under Load Tester supplier

LRC-03 ISO 3187 High Temperature Rul and Creep Tester Refractoriness Under Load Tester