Add to Cart
Frosted Milky White Frosted Perspex Sheet Custom 3mm Plastic Plate
3mm acrylic frosted sheet milky white perspex plastic plate cut to
size
1. How to use acrylic shadowless glue
1. Facade bonding Facade bonding is the most widely used bonding
technology. The surface to be bonded should be wiped clean first.
It is best to use a master to achieve bonding, so that the bonded
object does not shake, which is beneficial to improve the quality
of bonding. The plexiglass plate with a thickness of 3mm is bonded,
and the thin metal wire can be placed in it, and the bonding is
completed by capillary action, and the metal wire is pulled out
before the adhesive is cured. Or you can use tape to protect the
parts that do not need to be adhered, leave the parts where the
adhesive is coated with adhesive, and then put it diagonally into
the plexiglass plate to squeeze out the bubbles.
2. Plane bonding Plane bonding is a relatively special bonding
method. First, wipe the surface to be adhered clean and place it
horizontally, and pour an appropriate amount of adhesive on the
surface. Place one side of the other plexiglass plate diagonally in
contact with the plexiglass plate coated with the adhesive, and
then put it down evenly and slowly to drive out the air bubbles
from one side to complete the bonding.
3. Bevel bonding The bevel must use a 90-degree angle mold to
prevent the displacement of the bonded surface. The adhesive should
be applied evenly and slowly. The master form can only be removed
after it is completely cured.
4. Docking Put the two plexiglass plates to be docked horizontally
on the operating platform and close them, and stick a tape on the
bottom, leaving a gap no larger than 0.3mm wide for the application
of adhesive. Then use a syringe to inject the adhesive from one
side evenly and slowly from the gap until it is fully filled, and
remove the tape after it is completely cured.
Precautions
This product contains methacrylic acid and its ester monomers,
which are slightly irritating to the skin and eyes. If accidentally
splashed into the eyes, please rinse with plenty of water
immediately. If you still feel unwell, you must go to the hospital
for inspection;
The ideal thickness of the adhesive layer during bonding is
0.01-0.05mm, too thin or too thick will affect the bonding
performance.
Do not move the material back and forth when irradiated with
ultraviolet rays, otherwise it will easily cause the whitening of
the adhesive layer and the decrease of the bonding strength.
2.Parameter
Item | Place of Origin | Guangdong China |
Brand Name | XH (Acrylic sheet manufacturer) | |
Model Number | H-001 | |
Material | High quality Virgin MMA raw material | |
Specification | Thickness | 2mm-50mm |
Acrylic sheet Size | 2440x1220mm, 1220*1830mm, customized | |
Density | 1.2g/cm3 | |
Appearance | Color | Clear / Black / White / Blue / Red or customized |
Light Transmission | >92.8% | |
Surface | Double Polished | |
Process Available | Processing Type | Cast |
Process Service | Custom Cut to Size,laser dot,UV printing | |
Sample | Sample fee | Normal A4 size is free, just shipping fee |
Sample Time | Normal size, 2days | |
Customized sample | Fee and time will be discussed by both | |
Supply Capacity | Production Ability | 50000 Pieces per Month |
Stock | Regular size stock is sufficient | |
Lead time | 7-10 days after your order | |
Package | Acrylic sheet | Covered by PE film or craft paper on double sides |
Package | Wooden pallet | |
Package size | 2450mm*1250mm*700mm or customized | |
Package weight | About 2000kg per pallet or customized | |
Trading Terms | MOQ | 50 Pieces |
Main Market | All over the world | |
Shipping Port | Shenzhen/Guangzhou Port by Sea | |
Transportation | By sea/ Air/ Express/Railway | |
Trading Terms | FOB, EXW, CIF, CNF, FCA | |
Payment Terms | T/T,Western Union, Paypal | |
Using Tips | Storage | Far away from organic solvents |
Scratching | Sharp objects may scratch the surface | |
Temperature | Long time less than 85℃ | |
Cleaning | Clean with soft cloth or scrub with soap |
3. What glue is used to bond the acrylic sheet
Acrylic shadowless adhesive is used for bonding plastics and various materials with excellent bonding effect; high bonding strength, the damage test can achieve the effect of plastic body rupture; flexible formula, no internal stress cracking phenomenon after curing , Excellent resistance to low temperature, high temperature and high humidity; fast curing speed, positioning in a few seconds, reaching the highest strength in one minute, greatly improving work efficiency; completely transparent after curing, the product will not yellow or whiten for a long time; compared with traditional Instantaneous adhesive bonding has the advantages of resistance to ring testing, no whitening, and good flexibility; it can be dispensed by automatic mechanical glue or screen printing, which is convenient for operation. Methyl chloride is just "chloroform", which is generally used for bonding. Available in chemical stores
4. XH Company and Production Line
5. Package and shipping
7.1. One piece of acrylic sheet package: double-sided covered with
kraft paper or PE film, the cover film does not have any LOGO of
our company.
7.2. Tray package: the total weight of each pallet is about 2 tons,
the bottom is wooden pallet or iron pallet, and the surrounding is
packed with corrugated paper.
7.3. The packaging method of the whole container: 20-23 tons (about
3000 pieces) 20-foot container, 10-12 pallets.