Brand | BWIN |
Model | Wcmt050308 Wcmt06t308 Wcmt080412 |
Color | Fuchsia/Black |
Workpiece | Steel/Stainless steel |
Type | U Drill CNC Carbide Inserts |
Material | Tungsten Carbide U Drilling Insert |
Processing | Medium Cutting |
Feature | High wear resistance |
High finish | |
Strong universality | |
Impact resistance | |
Stable performance | |
Standard | ISO |
Quantity | 10pcs/box |
Weight | 0.015kg |
Package | Plastic Box |
Customized | OEM, ODM |
Lead Time:
antity(pieces) | 1 - 3000 | >3000 |
Lead time (days) | 7 | To be negotiated |
Notice:
Applications:
Our cnc U drill insert could to be processed Alloy steel, Tool steel, carbon steel, stainless steel, Cast iron and Titanium alloy. Working material as following:
Advantage
1. Distribution and wholesale, complete in variety
Large quantity is preferred, product specifications are complete, and the pattern is subdivided into processing technology levels to meet your processing needs for different angles and different workpieces;
2. Carefully selected materials with reliable quality
Every detail has been strictly checked, and better products have been meticulously created. They are cheap, stable, durable and have a long service life
3. Sufficient supply and large inventory
We have our own factory, with a large amount of inventory to provide you with sufficient supply, so you don't need to worry about the shortage crisis, so that you can use it with confidence. Support customization, large quantity and price can be discussed, welcome to consult.
4. After sales service
We have a complete after-sales system. Cooperation is not the end, it is the beginning. If you have after-sales problems, please contact us at any time, and we will solve them for you as soon as possible.
1. Flank Wear? Higher cutting resistance,Notch wear on flank,Poor
roughness of surface, or deterioration of accuracy.
Soft grades,Excessive cutting speed,Small flank angle,Low feed.
Select a higher,wear-resistant grade,Reduce cutting speed,Increase
flank angle,Increase feed.
2. Crater Wear? Uncontrolled chip,Poor surface quality,when
finishing High speed processing carbon steel
Soft grades,Excessive cutting speed,Excessive feed,The strength of
chip breaker Insufficiet.
Change to a higher wear-resistant grade,Reduce cutting speed,Reduce
feed,Select a higher strength chip breaker.
3. Chipping? Sudden fracture of cutting edge(rake face and
flank),Instability insert life
Toughness insufficient,Excessive feed rate,Strength of cutting edge
insufficient,Instability of the tool.
Select a tougher grade,Decrease feed rate,Increase honing of
cutting edge(chamfering to rounding),Increase the stability and
setting angle
4. Insert Fracture? Cutting resistance increased Poor surface
roughness.
Toughness insufficient,Excessive feed rate,Strength of cutting edge
insufficient,Instability of the tool.
Select a tougher grade,Decrease feed rate,Increase honing of
cutting edge(chamfering to rounding),Increase the stability and
setting angle.
5. Plastic Deformation? Variation of dimension Nose wear,cutting
edge drape or passivating.when processing alloy steel Poor surface
roughness
Soft grade,Excessive cutting speed,Excessive cutting depth and feed
rate,Overheat on cutting edge.
Select a higher red hardness cutting material,Decrease cutting
speed,Decrease cutting depth and feed rate,Select a higher thermal
conductivity cutting material(CVD+sufficient coolant).
6. Build-Up-Edge? Workpiece dissove with Cutting edge Poor surface
roughness when finishing,Cutting resistance increased,Cutting soft
materials.
Cutting speed too low,Cutting edge obtuse,Unsuitable tool material.
Increase cutting speed,Increase rake angle,Select small sticking
force.