Product Details
GH3536 Nickel Based Solid Solution Reinforced Superalloy Hastelloy
X
GH3536 is a Nickel Based Solid Solution Reinforced Superalloy. It
is equal to Hastelloy X alloy.
It has good resistance to oxidation and corrosion resistance, under
900 ℃ have moderate to lasting and creep strength, cold and hot
working good formability and weldability.
Applicable to the manufacture of aircraft engine combustion chamber
components and other high temperature parts, use for a long time
under 900 ℃, short-time working temperature of 1080 ℃. In 600 ~
1200 ℃ high temperature can withstand the stress and resistance to
oxidation and corrosion resistance of the alloy. The matrix
elements can be divided into iron base superalloy, nickel base
superalloy and cobalt base superalloy. According to the preparation
process, it can be divided into deformation superalloy, casting
superalloy and powder metallurgy superalloy. According to the
reinforcement method, there are solid solution enhancement,
precipitation enhancement, oxide dispersion enhancement and fiber
enhancement (see metal enhancement). High temperature components
such as turbine blades, guide blades, turbine discs, high-pressure
compressors and combustors for aerospace, naval vessels and
industrial gas turbines. It is also used in the manufacture of
energy conversion devices such as space vehicles, rocket engines,
nuclear reactors, petrochemical equipment and coal conversion
Chemical composition
| Element | C | Cr | Ni | Co | W | Mo | Al | Ti |
| Weight(%) | 0.05~0.15 | 20.50~23.00 | Rem | 0.50~2.50 | 0.20~1.00 | 8.00~10.00 | 0.50 max | 0.15 max |
| Element | Fe | B | Mn | Si | P | S | Cu | |
| Weight(%) | 17.00~20.00 | 0.010 max | 1.00 max | 1.00 max | 0.025 max | 0.015 max | 0.500 max | |
Characters of GH3536
- Good workability.
- At 900 ℃ with medium of lasting and creep strength.
- Good oxidation resistance and corrosion resistance.
- Suitable for application in a long time of aircraft engine
combustor under 900 ℃ and reheater components.
- Good welding performance and cold and hot working formability.
Application of GH3536
- Industrial and aircraft steam turbine (burner, rectifier,
structural cover)
- Industrial furnace components, supporting roller, grid plate,
ribbon and radiation pipe
- Spiral pipes in a petrochemical furnace
- High temperature gas cools the nuclear reactor
Forms and sizes of supply
Plate 0.50~4.0mm
Strip: 0.05~0.80mm
Tube: diameter 4~20mm, wall thickness 1.0~2.0mm
Wire: diameter 0.20~10.00mm
Bar: diameter upto 300mm
Company Profile
Suzhou Xunshi New Material Co., Ltd (refered as Xunshi afterwards) is a professional supplier of high performance alloys. Our factory
is specialized in manufacturing Nickel alloys & Cobalt alloys for
10+ years,with a company mission to provide a high quality, reliable
source for precision alloys, high temperature alloys and stainless
steels in both pilot run and mass production. We are professionally
manufacturing materials with unique features, which are then used
in aerospace, military, electronics, marine, petroleum and
petrochemical industries.
Base on “Quality-oriented, Leading Technology, Continuous
Improvement, Customer Satisfaction”, we believe Xunshi could be
your best supplier.
Product Scope of Xunshi
· Inconel
· Hastelloy
· Incoloy
· Monel
· Nimonic
· Nitronic
· Haynes
· Special Stainless Steel
· Soft Magnetic Alloy
· Permanent Magnetic Alloy
· Elastic Alloy
· Controlled Expansion Alloy
· Magnetostrictive Material
Services of Xunshi
· Material selection
· Non-standard product research and pre-production
· Hard to find material sourcing
· Cutting/splitting
· Precision machining
· Heat treatment
· Customized Packing
· Logistics service
Advantages of Xunshi
· Experienced in industry
· Quality control system
· Authorized Certificates
· Guaranteed delivery and quality
· Customers from 30+ countries trust us
Xunshi is engaged in introducing China-origin high performance alloys to
the entire world. Choose Xunshi, choose high performance.