Condensers Coated Copper Pipe , Stress Corrosion Resistant Copper Gas Pipe

Brand Name:TOBO
Certification:SGS /TUV/BV
Model Number:C71500
Minimum Order Quantity:1 PCS
Delivery Time:10-20 WORKDAYS
Payment Terms:L/C, D/A, D/P, T/T, Western Union, MoneyGram
Contact Now

Add to Cart

Verified Supplier
Location: Shanghai Shanghai China
Address: No.208,Lvdi Road,Baihe Town,Qingpu District,Shanghai,China
Supplier`s last login times: within 34 hours
Product Details Company Profile
Product Details

Condensers Coated Copper Pipe , Stress Corrosion Resistant Copper Gas Pipe


Copper Nickel C715 - C71500


C715 Cupro-Nickel is a 70/30 copper nickel alloy that is almost entirely resistant to stress corrosion.


ASTM B151, ASTM B466, ASTM B111, ASTM B171, ASME SB466, ASME SB111, ASME SB151, ASME SB171, DIN 2.0872, BS 2871 CN102, EN CW352H, MIL-C-1726F, MIL-C-24679, MIL-T-16420K


C71500 COPPER NICKEL APPLICATIONS

  • Copper nickel alloy 715 finds its greatest application in areas of high temperatures and pressures combined with high velocity and destructive turbulence. The small iron content, up to 0.5%, gives the C715 alloy an extraordinary resistance to general corrosion and stress corrosion cracking, making it very suitable and ideal for the marine or industrial industries.

    Common applications include:

  • Condensers
  • Seawater piping
  • Power plants
  • Exchanger shells

C71500 Copper Nickel Specifications


End ProductSpecification
BarASTM B151, B122, MILITARY MIL-C-15726
Pipe, SeamlessASME SB466, ASTM B466
Pipe, WeldedASME SB467, ASTM B608, B467
PlateASTM B122, MILITARY MIL-C-15726
Plate, CladASTM B432
Plate, Condenser TubeASME SB171, ASTM B171, SAE J463, J461
RodASTM B151, MILITARY MIL-C-15726
Rod, WeldingAWS A5.15
SheetASTM B122, MILITARY MIL-C-15726, SAE J463, J461
StripASTM B122, MILITARY MIL-C-15726
Tube, CondenserASME SB111, ASTM B552, B111, MILITARY MIL-T-15005, SAE J463, J461

LIST OF STANDARD C71500 SIZES


Round Bar: ¼” Dia. thru 10”


Sheet:065”, .125”


Plate:3/16” thick thru 3”


Tube: Condenser tube


Pipe:¼” Standard (SCH 40) thru 10”


¼” Extra Heavy (SCH 80) thru 4”


½” Class 200 Mil-T-16420 K thru 10”


Fittings: Class 200, SCH 40, SCH 80, Butt-weld Fittings


Threaded and Socket-weld Fittings, 3000#/6000#


C96200 400# Socket-weld Fittings


Flanges: Slip-on, threaded, blind, Weld-neck Flanges


Ameritube has been providing C71500 Copper Nickel 70/30 according to the following standards:

  • ASME SB-111
  • ASME SB-466
  • ASTM B-111
  • ASTM B-466
  • MIL-T-15005f
  • MIL-T-16420k Class 200, 700, 1650, 3300, and 6000

Typical Uses for C71500 Copper Nickel "70/30":

AUTOMOTIVE: Power Steering Tube, Brake Lines


CONSUMER: Screw Lamp Bases


INDUSTRIAL: Condenser Plates, Condensers, Weld Torch Tips, Heat Exchanger Tubes, Valve Bodies,

Evaporator Tubes, Pressure Vessels, Distiller Tubes, Pump Impellers for Oil Refining, Ferrules, Evaporators


MARINE: Boat Hulls, Tube Sheet for Salt Water Service, Salt Water Pipe Fittings, Salt Water Piping Systems, Salt Water Piling Wrap, Hot Water Tanks, Salt Water Baffles, Propeller Sleeves, Ship Hulls, Water Hoses


Equivalencies Copper Nickel (70/30) tube/pipe


KS D5301

JIS H3300

C7060T
ASTM B111C70600
ASTM B466C70600
BS2871 {PART2}CN102
AS1752C70600
DIN17664CuNi10Fe 1Mn
DIN 86019 WL2.1972CuNi10Fe 1.6Mn
EEMUA 1447060X
MIL-T-16420K706
EN12449CW352H

PLUMBING: Flanges


Brand Name:TOBO
Model Number:90/10 Copper nickel alloy
Certification:SGS/BV/ABS/LR/TUV/DNV/BIS/API/PED
Place of Origin:China

PICTURES:



FAQ.

Q: Are you trading company or manufacturer ?
A: We are manufacturer ,You can see the certification.

Q: How long is your delivery time?
A: Generally it is 5-10 days if the goods are in stock. or it is 15-20 days if the goods are not in stock, it is according to quantity.

Q: Do you provide samples ? is it free or extra ?
A: Yes, we could offer the sample for free charge but need pay the cost of freight.

Q: What is your terms of payment ?
A: Payment<=1000USD, 100% in advance. Payment>=1000USD, 50% T/T in advance ,balance before shippment.

China Condensers Coated Copper Pipe , Stress Corrosion Resistant Copper Gas Pipe supplier

Condensers Coated Copper Pipe , Stress Corrosion Resistant Copper Gas Pipe

Inquiry Cart 0