Chemical Composition ( For Reference Only )
Alloy | Si | Fe | Cu | Mn | Mg | Zn | Cr | Ti | code |
8011 | 0.5-0.9 | 0.6-1.0 | 0.1 | 0.2 | 0.05 | 0.1 | 0.05 | 0.08 | 1 |
3003 | 0.6 | 0.7 | 0.05-0.2 | 1.0-1.5 | - | 0.1 | - | - | 2 |
5052 | 0.25 | 0.4 | 0.1 | 0.1 | 2.2-2.8 | 0.1 | 0.15-0.35 | - | 3 |
1060 | 0.25 | 0.35 | 0.05 | 0.03 | 0.03 | 0.05 | - | - | 4 |
1145 | Si+Fe:0.55 | 0.05 | 0.05 | 0.05 | - | - | 0.03 | 5 | |
3A21 | 0.6 | 0.7 | 0.2 | 1.0-1.6 | 0.05 | 0.1 | - | 0.15 | 6 |
Mechanical Performance ( For Reference Only )
Temper | Tensile Strength Rm(MPa) | Yield Strength Rp0.2(Mpa) | Extend Ratio A50(%) |
O | 80- 110 | 20 | 6.0 |
H22 | 100 - 135 | 16 | 5.5 |
H24 | 115 -145 | 12 | 5.0 |
H26 | 125 - 160 | 8 | 4.0 |
H18 | 160 | 1 | - |
Hydrophilic Foil Coating Layer Performance
S/N | Item | Technical data |
1 | Film Thick ness | 1.0-2.0um ( single side average thickness) |
2 | Hydrophilicity | Primary contact angle? o Continuous contact angle? 20o |
3 | Adherencce Strength | Erichsen test ( pressed depth 5mm ), no peeling off. Gridding test (100 / 100 ) : No separating |
4 | Corrosion Resistance | Salt & Spray test ( 72 hours ) : R . N ? 9.5 |
5 | Alkai resistance | Dipped in 20o% Na OH under 20oC for 3 minutes, absolutely no blister |
6 | Impregnant resistance | Sample weight loss ? 1 % |
7 | Heat resistance | Under 200oC keep 5 minutes, performance and colo unchanged Under 300oC keep 5 minutes, coating film become a bit yellow |
8 | Oil proof | 24 Hours, no blister on the coating layer |
9 | Coating film odor | No strange odor |