Alloy Hastelloy C-4 UNS NS355 N06455 Hastelloy Plate Chemical Resistant

Brand Name:MITTEL
Certification:SGS ISO MTC
Model Number:Hastelloy C-4
Minimum Order Quantity:50KGS
Delivery Time:14 Days
Payment Terms:L/C, T/T
Contact Now

Add to Cart

Verified Supplier
Location: Wuxi Jiangsu China
Address: NO.288,YOUYI ROAD ,XI SHAN DISTRICT,WUXI CITY,CHINA
Supplier`s last login times: within 48 hours
Product Details Company Profile
Product Details
Material

Hastelloy C4 Nickel Alloy ASTM B619 B622 B626 N06455 N06455 Nickel Alloys Plate





Hastelloy C4 ASTM B619 B622 B626 N06455 N06455 Nickel alloy is a nickel-chromium-molybdenum alloy with outstanding high-temperature stability as evidenced by high ductility and corrosion resistance even after aging in the 1200 to 1900°F (649 to 1038°C) range. This alloy resists the formation of grain-boundary precipitates in the weld heat-affected zone, thus making it suitable for most chemical process applications in the as welded condition. C-4 alloy also has excellent resistance to stress-corrosion cracking and to oxidizing atmospheres up to 1900°F (1038°C).

Hastelloy C4 ASTM B619 B622 B626 N06455 N06455 Nickel alloy has exceptional resistance to wide variety of chemical process environments. These include hot contaminated mineral acids, solvents, chlorine nd chlorine contaminated media (organic and inorganic), dry chlorine, formic acid and acetic acid, acetic anhydride, and seawater and brine solutions.

Hastelloy C4 ASTM B619 B622 B626 N06455 N06455 Nickel alloy can be forged, hot-upset, and impact extruded. Although the alloy tends to work-harden, it can be successfully deep-drawn, spun, press formed or punched. All of the common methods of welding can be used to weld Hastelloy C4 ASTM B619 B622 B626 N06455 N06455 alloy, although the oxy-acetylene and submerged arc processes are not recommended when the fabricated item is intended for use in corrosion service. Special precautions should be taken to avoid excessive heat input.

Hastelloy C4 ASTM B619 B622 B626 N06645 Nickel Alloy Chemical compostion:

ASTM B622 N06645 Hastelloy C4 Nickel Alloy Chemical Composition:

NiMoFeCCoCrMnSiTiWAlCuVPSZrNbTa
Rem.14.0- 17.03.0 max0.015 max2.0 max14.0- 18.01.0 max0.08
max
0.70 max1.0 max0.04 max0.03 max

DIN 17744 2002 2.4610 NiMo16Cr16Ti Hastelloy C4 Nickel Alloy Chemical Composition:
NiMoFeCCoCrMnSiTiWAlCuVPSZrNbTa
Rem.14.0- 17.03.0 max0.015 max2.0 max14.0- 18.01.0 max0.08
max
0.70 max0.50 max0.025 max0.015 max

Hastelloy C4 ASTM B619 B622 B626 N06645 Nickel Alloy Mechanical Properties:
DIN 17751 2002 2.4610 NiMo16Cr16Ti Hastelloy C4 Nickel Alloy Mechanical Properties
Material GradeMatrial NumberTensile Strength
Rm
N/mm²(MPa)
min
Yield Strength
Rp0.2%
N/mm²(MPa)
min
Yield Strength
Rp 1.0%
N/mm²(MPa)
min
Elongation
(%)
Brinell Hardness
HBW 2.5/62.5
maxApproximately
Hastelloy C42.461069027529540240-

ASTM B622 N06645 Hastelloy C4 Nickel Alloy Mechanical Properties
Material GradeMatrial NumberTensile Strength
Rm
N/mm²
ksi(MPa)
min
Yield Strength
Rp0.2%
N/mm²(MPa)
min
Elongation
(%)
Hastelloy B2N10665100 (690)40 (276)40

DIN 17751 2002 NiMo28 2.4617 Hastelloy B2 Nickel Alloy Specifications
Pipe SmlsWelded PipeTube SmlsWelded TubeSheet/PlateBarForgingFitting
B622B619B622B626B333B335B564B366

Hastelloy C4 Nickel Alloy DIN 17751 2.4610 ASTM B619 B622 B626 N06645 Specification:
StandardsDesciption
ASTM B574Standard Specification for Low-Carbon Nickel-Chromium-Molybdenum, Low-Carbon Nickel-Molybdenum-Chromium, Low-Carbon Nickel-Molybdenum-Chromium-Tantalum, Low-Carbon Nickel-Chromium-Molybdenum-Copper, and Low-Carbon Nickel-Chromium-Molybdenum-Tungsten Alloy Rod
ASTM B575Standard Specification for Low-Carbon Nickel-Chromium-Molybdenum, Low-Carbon Nickel-Chromium-Molybdenum-Copper, Low-Carbon Nickel-Chromium-Molybdenum-Tantalum, Low-Carbon Nickel-Chromium-Molybdenum-Tungsten, and Low-Carbon Nickel-Molybdenum-Chromium Alloy Plate, Sheet, and Strip
ASTM B366Standard Specification for Factory-Made Wrought Nickel and Nickel Alloy Fittings
ASTM B564Standard Specification for Nickel Alloy Forgings
ASTM B619Standard Specification for Welded Nickel and Nickel-Cobalt Alloy Pipe
ASTM B622Standard Specification for Seamless Nickel and Nickel-Cobalt Alloy Pipe and Tube
ASTM B626Standard Specification for Welded Nickel and Nickel-Cobalt Alloy Tube
ASTM B704Standard Specification for Welded Alloy Tubes
ASTM B705Standard Specification for Nickel-Alloy Welded Pipe
DIN 17744 (2002/09)nickel-forgeable alloy with molybdenum and chrome
DIN 17750 (2002/09)ribbons and sheet metal out of nickel with nickel-wrought alloy properties
DIN 17751 (2002/09)tubes out of nickel with nickel-wrought alloy properties
DIN 17752 (2002/09)rod made from nickel with nickel-wrought alloy properties
DIN 17753 (2002/09)wire out of nickel with nickel-wrought alloy properties
VdTÜV / Werkstoffblatt 432/1extremely corrosion resistant nickel based alloy, niCr21Mo, material-nr. 2.4858 ribbon, sheet metal
VdTÜV / Werkstoffblatt 432/2432/2 extremely corrosion resistant nickel based alloy, NiCr 21 Mo, material-nr. 2.4858 seamless pipe
VdTÜV / Werkstoffblatt 432/3extremely corrosion resistant nickel based alloy, NiCr 21 Mo, material-nr. 2.3858 rod steel, forging

Hastelloy C4 ASTM B619 B622 B626 N06455 N06455 Applications
This alloy is used to manufacture chemical process equipment, especially for process use at high temperatures where stainless steel do not have adequate strength and/or corrosion resistance.

Machinability
Machinable by conventional techniques.

Forming
Readily formed by conventional methods.

Welding
All of the common methods of welding apply to this alloy. However excessive heat input should be avoided and submerged arc or oxy-acetylene welding should not be used as they can degrade corrosion resistance.

Heat Treatment
Solution annealed at 1950 F and rapid quench. This is the normal condition in which product forms are supplied.
Forging
The alloy can be hot forged at temperatures of 2150 F to 1750 F.

Hot Working
Can be hot worked or hot extruded similar to stainless steels.

Cold Working
Readily cold worked by conventional means.

Annealing
Solution anneal at 1950 F followed by rapid quench.

Aging
May be aged (after solution heat treatment) at 1200 F for 10 hours to somewhat improve ductility and yield strength without adversely affecting the ultimate tensile strength.

Hardening
Hardened by cold working only, but normally used in the solution annealed condition .


Hastelloy C4 ASTM B619 B622 B626 N06455 N06455 Physical properties:
Density8.64 g/cm3
Melting point1350-1400°C

China Alloy Hastelloy C-4 UNS NS355 N06455 Hastelloy Plate Chemical Resistant supplier

Alloy Hastelloy C-4 UNS NS355 N06455 Hastelloy Plate Chemical Resistant