Add to Cart
ASME SA213 T12 HFW FIN TUBE FOR BOILER AND HEAT EXCHANGER
ASME SA213 T12 is a specification for seamless ferritic alloy steel
boiler, superheater, and heat exchanger tubes. HFW (High Frequency
Welding) fin tubes are a type of finned tubes that are manufactured
using high-frequency electric resistance welding. These fin tubes
are used in boilers and heat exchangers to enhance heat transfer
efficiency.
The combination of ASME SA213 T12 tubes and HFW fin tubes provides
several benefits for boiler and heat exchanger applications. The
T12 alloy steel offers excellent mechanical properties, high
temperature strength, and corrosion resistance, making it suitable
for high-pressure and high-temperature environments.
The HFW fin tubes have fins that are welded onto the base tube
using high-frequency electric resistance welding. This welding
technique ensures a strong bond between the fins and the tube,
resulting in improved heat transfer efficiency. The fins increase
the surface area of the tube, allowing for better heat exchange
between the fluid inside the tube and the surrounding environment.
Overall, the use of ASME SA213 T12 HFW fin tubes in boilers and
heat exchangers helps improve the overall performance and
efficiency of these systems, leading to cost savings and better
energy utilization.
Chemical Components (%) | |||||||
Grade | C | Mn | P | S | Si | Cr | Mo |
T11 | 0.05-0.15 | 0.30-0.60 | ≤0.025 | ≤0.035 | 0.50-1.00 | 1.00-1.50 | 0.44-0.65 |
T12 | 0.05-0.15 | 0.30-0.61 | ≤0.025 | ≤0.035 | 0.5 | 0.80-1.25 | 0.44-0.65 |
T22 | 0.05-0.15 | 0.30-0.60 | ≤0.025 | ≤0.035 | 0.5 | 1.90-2.60 | 0.87-1.13 |
Grade | UNS Number | Heat Treat Type | Subcritical Annealing or Tempering Temperature, Min or range °F [°C] |
T11 | K11597 | full or isothermal anneal normalize and temper | 1200 [650] |
T12 | K11562 | full or isothermal anneal normalize and temper subcritical anneal | 1200 to 1350[650 to 730] |
T22 | K21590 | full or isothermal anneal normalize and temper | 1250 [675] |
Mechanical properties | ||||
Grade | Tensile | Yield | Elongation | Hardness |
Strength (Mpa) | Strength (Mpa) | (%) | (HRB) | |
T11 | ≥415 | ≥220 | ≥30 | ≤85 |
T12 | ≥415 | ≥220 | ≥30 | ≤85 |
T22 | ≥415 | ≥220 | ≥30 | ≤85 |
Application