CCCW-C cementitious capillary crystalline waterproofing coating

CCCW-C cementitious capillary crystalline waterproofing coating

Country/Region: china
Company: Panjin Yuwang Waterproof Building Materials Group
Categories: Anti Corrosion Coatings
Update: 2016-05-12 11:31:56
ICP License: Issued by the Chinese Ministry
Panjin Yuwang Waterproof Building Materials Group
ICP Remarked Supplier
China
Business type:
Supplier`s last login times: within 40 hours

View larger image

CCCW-C cementitious capillary crystalline waterproofing coating

Product Specifications:
Implementation of the standards:
Views:52
Manual Download

Products

Product Overview

Based on Portland cement, silica sand and various active chemicals developed from a rigid waterproof material. After the interaction with water, the material of the active chemical substance by the carrier to penetrate the concrete to form insoluble in water in concrete
Crystals, filling pores Road, preventing concrete cracking, reinforced concrete strength, prevent steel corrosion and chemical resistance, and thus have a permanent waterproof effect, is a non-toxic, tasteless, non-polluting environmentally friendly products.
Code tag
CCCW- cementitious capillary crystalline waterproofing materials; C- cementitious capillary crystalline waterproofing coating.
Order by product name and standard number of tags.
Example: cementitious capillary crystalline waterproofing coating labeled: CCCW C GB 18445-2012
Implementation of the standards
GB 18445-2012 "cementitious capillary crystalline waterproofing materials."
Features
highly resistant to pressure capability, strong penetration ability, long-term ability to repair itself.
has a unique breathing, anti-corrosion, anti-aging, protect steel capacity.
environmentally friendly, non-toxic, excellent compatibility with other materials.
construction method is simple, labor-saving.
Construction Method
Can be painted or dry sprinkle method.
Brushing Construction Method:
Primary treatment: Requires a solid, flat, non-clear water, no dust, no oil, and grass-roots fully wetted.
Ingredients: Ingredients mass ratio, the ratio of powder: water = 1: 0.4-0.5. It is appropriate mechanical mixing, stir to form a viscous slurry water.
Brushing: The preparation of a good material to be not less than 1.5kg / m2 amount of brushing the grass-roots level, the second time the coating can be painted over in first coat is still wet; also available in the first pass coating after the floor is completely dry before the first pass pre-wet coating, and then a second time brushing.
Conservation: You must use water, use spray after the initial setting, be sure to avoid the coating is damaged. It normally takes water three times a day for 2-3 days, and on a hot day or dry weather to be several times more spray to prevent premature drying coating. Curing process, within 48 hours to avoid anti-rain, frost, sun, wind, water and low temperature 2or less. After the concrete structure containing liquid (such as swimming pools, reservoirs, water storage tank, etc.) must be 3 days of conservation, then place 12 days before coming down the liquid. Costumes extremely hot or corrosive liquids concrete structures, the need to put 18 days before filling Sheng.
Construction Points:
base layer must be sufficiently wetted, the dried base surface, the sprinkler to be processed to meet the requirements.
must protect the coating amount not less than the amount per square meter of 1.5 kg.
maintenance work must be done, need to strictly implement the provisions.
The above three points, capillary crystalline waterproofing coating ensure the necessary conditions for full waterproof effect.
Dry sprinkle Construction Method:
Dry sprinkle method of construction can be in two locations:
Before pouring the concrete floor for half an hour, the cushion surface dry shake. The mat wetted with water, and then screen or hands evenly sow powder, then promptly poured concrete floor.
In the not fully cured concrete surface sown dry. Sprinkle dry hand or sieve the powder directly sown thereon immediately with a trowel, the powder is pressed into the grinder concrete and calendering.
Dosage: coating, paint 1.0mm total amount of not less than 1.5kg / m2.
Applications
Widely used in cement mortar, old and new concrete buildings and structures in welcoming classes and dorsal surface water. Such as: basement, subway, bathroom, kitchen, reservoirs, swimming pools, storage buildings, culverts, concrete pavement and so on.
Packaging Storage
Packaging: iron sealed package, 20kg / barrel.
Storage: Store in a dry place, is strictly prohibited open storage of different types are stored, is strictly prohibited damp, from the date of production storage period of one year.
Transportation: upright; prevent the sun and rain; to prevent collisions, keep the packaging intact; light handling, may not throw throw.


Product Tags:

cementitious waterproofing coating

      

concrete crystalline waterproofing

      

powder coat curing

      

CCCW-C cementitious capillary crystalline waterproofing coating Images

Send your message to this supplier
From:
Enter your email please.
To: Panjin Yuwang Waterproof Building Materials Group
Subject:
Message:
Characters Remaining: (0/3000)
 
Inquiry Cart 0
Other about

CCCW-C cementitious capillary crystalline waterproofing coating

CCCW-C cementitious capillary crystalline waterproofing coating

Categories :Anti Corrosion Coatings
Update :2016-05-12 11:31:56

801 water-cement construction adhesive

Categories :Cement Based Waterproofing
Update :2016-05-12 11:31:57

FD-324 water leak

Categories :Water Resistant Labels
Update :2016-05-12 11:31:57

P-333 asphalt shingles special glue

Categories :Water Resistant Labels
Update :2016-05-12 11:31:58

FMJ-338 highly viscous bitumen rubber coating

Categories :Coating Raw Materials
Update :2016-05-12 11:31:59

P-342 concentrated primer

Categories :Waterproof Sun Protection
Update :2016-05-12 11:32:00